Hot Peel DTF Film Hot Selling Roll Hot Peel Dtf Pet Film Clear Dtf Pet Film for Dtf Printer

Material PET
Application DTF printing
Type Heat Transfer
Size A3,A4,A3+,30/33/60cm,custom
Peeling method: instant peeling
Microns 75μ
Packing 60cm*100m/roll, 9kg
Transfer Temp: 150-170℃
Transfer Time: 8-15 S
Application fields: sportswear, T-shirts, advertising shirts, group clothing, children’s clothing, luggage, shoes and hats,etc.

Material PET
Application DTF printing
Type Heat Transfer
Size A3,A4,A3+,30/33/60cm,custom
Peeling method: instant peeling
Microns 75μ
Packing 60cm*100m/roll, 9kg
Transfer Temp: 150-170℃
Transfer Time: 8-15 S
Application fields: sportswear, T-shirts, advertising shirts, group clothing, children’s clothing, luggage, shoes and hats,etc.

1. The pattern after transfer has a texture like PU glue. It has strong stretch resilience and does not deform. It feels softer than glue (30~50% softer than the pattern printed with oil-based coating film).
2. Adaptable to most inks on the market, 100% of the ink volume can be dispensed at will, without ink accumulation or bleeding.
3. The surface of the film is dry and can be sprinkled with 200 mesh ultra-fine powder without sticking to the powder. It can be easily torn hot, warm or cold.

Usage:
1. The surface with ink-absorbing coating is the printing surface;
2. Handle it with care and pay attention to the anti-scratch ink-absorbing coating;
3. Bake for 40 to 90 seconds after printing (adjust the appropriate temperature according to the performance of the hot melt powder);
4. Choose 60~80 mesh hot melt powder to achieve instant peel, 100~150 mesh hot melt powder is recommended for warm or cold peel, and 150 mesh or above hot melt powder is recommended for cold peel;
5. Store in a dry place and avoid moisture.

Notice:
If the baking temperature is too high or the baking time is too long after printing and sprinkling hot-melt powder, white spots may appear on the surface of the pattern. This is because the slow-drying agent in the ink cannot evaporate after the hot-melt powder is formed into a film. After the gas cools, it will form mist-like crystals on the surface of the pattern. This whitening phenomenon will slowly disappear after a few days of storage and contact with air, and will not affect the beauty of the pattern in the later stage.